BNI Preston CenterDallas, TX Visit a meeting

Painter · 7 min read

Elastomeric coating or regular exterior paint: which is right for stucco and masonry walls

Elastomeric coatings are thick, flexible and good at hiding hairline cracks, but they are not a cure for every wall. Here is how to choose between them and standard exterior paint.

Is elastomeric coating better than regular exterior paint?

Only for the right wall. I recommend elastomeric coating for sound concrete, block or stucco that has fine hairline cracks and good flashing, because the thick, flexible film bridges those cracks and sheds wind-driven rain. On walls that need to dry, or that leak for another reason, a breathable acrylic masonry paint is usually the better and safer choice.

I'm Andrey Shelokovskiy, and we at Nomad Painting and our commercial arm, Nomad Coatings, paint homes and commercial buildings across Dallas–Fort Worth. Before I came to this work I spent six years at PPG Protective and Marine Coatings, and I am a member of NACE, the corrosion engineers' association. Coating selection is the part of the job I enjoy most, because the wrong system fails no matter how well it is applied.

This guide explains what elastomeric coating actually is, where it earns its higher cost and where it causes problems, so you can read a proposal for a stucco or masonry building with a sharper eye.

What elastomeric coating actually is

Elastomeric coating is a high-build, flexible acrylic film, applied much thicker than paint, that stretches as a wall moves. Sherwin-Williams describes its ConFlex SherLastic elastomeric coating as one that covers and hides hairline cracks, elongates, resists efflorescence and protects exterior concrete and masonry against wind-driven rain.

Regular exterior acrylic paint forms a thinner film. It still flexes a little, and good masonry paints resist alkali and weather well, but it will not span a crack that opens and closes with the seasons. A hairline crack under standard paint usually telegraphs back through within a season or two.

Elastomeric is also not one product. Manufacturers sell smooth and textured versions, versions made for concrete and masonry, and versions made for metal roofs, each with its own data sheet listing approved surfaces, primers, temperatures and coverage. When a proposal simply says elastomeric, ask for the product name, so you can read what the manufacturer says it is made for.

The thickness that makes elastomeric useful also changes how the wall handles moisture. That trade-off, not the price, is what should drive the decision.

Why breathability decides most of the choice

Masonry and stucco walls take on water from rain, from the ground and from inside the building, and that water has to leave as vapor. A coating that lets vapor pass is called breathable or vapor permeable.

The Northwest Wall and Ceiling Bureau, a trade association for wall and stucco contractors, recommends painting cement stucco with a breathable product designed for it. Its technical guidance notes that elastomeric coatings are typically very low in vapor permeability and can trap moisture trying to leave the wall, and it suggests paints and coatings with a perm rating of 7 or higher.

Building Science Corporation documented what happens when the balance goes wrong. On a 1920s masonry building, rain entered through poorly detailed parapet caps faster than it could dry through the elastomeric coating, and the coating blistered. The coating was the symptom; the parapet was the cause. I explain the same principle for brick in our guide on paint, limewash or mineral paint for a brick house.

When does elastomeric coating make sense?

Elastomeric coating makes sense when the wall is structurally sound, the water is coming from outside through fine cracks, and the flashing and drainage are already in good shape. The NWCB notes that elastomerics have worked well on stucco systems with good flashings and drainage.

The situations where I usually propose it:

Before I write elastomeric into a proposal, I walk the building with the owner or property manager and look at the places water usually gets in: window perimeters, roof-to-wall joints, parapet caps, sealant joints and downspout outlets. If those are sound and the cracking is fine and widespread, elastomeric is often the most durable answer for that wall.

  • Concrete block or tilt-up walls on a warehouse or retail building with a network of hairline cracks.
  • Stucco with fine map cracking where water stains appear inside after storms with wind-driven rain.
  • Masonry walls facing the prevailing weather that keep absorbing rain through the surface.
  • Buildings where the owner wants a long repaint cycle and the wall has been inspected for leaks at windows, roof edges and parapets.
  • Surfaces the coating manufacturer lists for that product, prepared and primed the way the data sheet requires.

When should you use regular masonry paint instead?

Use a breathable acrylic masonry paint when the wall needs to dry, when the cracks are structural or active, or when the real problem is a leak somewhere else. The NWCB says plainly that an elastomeric coating should not be used to solve a water intrusion or flashing problem.

Regular paint is usually the better fit in these cases:

Choosing regular paint is not settling for less. A breathable, alkali-resistant acrylic masonry paint applied over a properly cleaned, patched and primed wall gives a sharp finish, lets the wall dry and is far easier to repaint in a new color later. For many homes and smaller commercial buildings, that is the better long-term system.

  • Older stucco or masonry that already shows blistering, efflorescence or moisture staining from inside.
  • Walls with leaks at windows, roof-to-wall joints, parapet caps or sealant joints that have not been fixed.
  • Wide or moving cracks that point to settlement; those need repair or an engineer's opinion, not a thicker coating.
  • Homes where the owner expects to change the color in a few years; the NWCB notes elastomerics can be difficult to remove or recolor.
  • Detailed trim, smooth siding and wood, where a heavy film looks out of place.

What North Texas weather does to both

Exterior coatings in North Texas deal with intense sun, high summer heat, wind-driven spring storms and the occasional hard freeze. On commercial work, I see heat, UV exposure, storms, dust and rain show up as fading, cracking, peeling and moisture problems.

Heat and sun make the flexibility of an elastomeric useful on walls that expand and contract every day. The same conditions make application timing critical, because a thick film applied in direct afternoon sun can skin over before it cures properly. Our guide on when to paint a house exterior in Dallas–Fort Worth covers temperatures, wind and season.

A hard freeze is where trapped moisture does the most damage. Water held behind a low-permeability film can freeze, expand and push the coating off the wall. That is one more reason I insist on finding and fixing water sources before any coating goes on.

Preparation matters more than the product

Neither coating will hold on a dirty, chalky or damp wall. Our exterior process for stucco, brick and masonry starts with washing, then scraping and sanding loose material, patching, caulking and priming, with surrounding areas protected before any coating goes on.

For elastomeric work, preparation also means treating cracks according to their size: hairline cracks can be bridged by the coating, while larger cracks are routed and filled with a compatible patching or sealant product first. New stucco needs time to cure as well. The NWCB notes new stucco is highly alkaline and recommends an alkali-resistant paint once the surface pH has dropped, which typically takes a week to 10 days.

If an existing coating is peeling, it has to come off down to a sound surface first. Our guide on what peeling and chalking exterior paint is telling you explains how to read the failure before you choose the next system.

Film thickness is the last part of preparation that owners rarely see. A thick coating applied too thin behaves like an expensive paint and loses its crack-bridging benefit. On any elastomeric job, the crew should follow the manufacturer's coverage rate and check film build as it goes, rather than stretching the material to cover more wall.

Cost, coverage and how long each lasts

Elastomeric coating usually costs more per wall than paint, because the material is applied much thicker, covers less area per gallon and takes more labor. The extra cost pays off when the wall truly needs crack bridging and weather resistance; on a wall that does not, it buys a heavier film and nothing else.

When you compare two proposals for the same stucco or block building, line them up on the same points: the product name for each surface, the primer, the number of coats, the planned coverage, the crack repair method and what happens at sealant joints and around windows. A lower bid that leaves out crack repair or primes only spots is not the same system at a better price.

How long either lasts depends far more on preparation, film thickness and water control than on the label. We say a properly prepped exterior should last 7 to 10 years, and that holds only when the moisture sources are handled. Our guide on what drives the cost of painting a house in Dallas–Fort Worth breaks down the line items that move an exterior quote.

Getting a coating recommendation for your building

Every commercial project starts with a site walk. We review the property, the exterior surfaces, access points, the current coating condition, business hours and your goals, then recommend a system for each surface: elastomeric, waterproofing, corrosion-resistant or standard paint, with the reasons written down.

You receive a detailed, itemized quote with no hidden fees, the same crew from start to finish and a final walkthrough with the project manager. We are fully insured with general liability and workers' compensation, and our work carries a two-year limited warranty on labor and materials.

If you manage a stucco or masonry building anywhere from Dallas to Frisco or Southlake, send photos of the cracks and any interior water stains before the visit. Those two things usually tell me which direction the recommendation will go.

Questions people ask me

Can elastomeric coating stop a wall from leaking?

Elastomeric coating can keep wind-driven rain from soaking through sound masonry with hairline cracks, but it is not a leak repair. Leaks at windows, roof edges, parapet caps or failed sealant joints need to be fixed at the source. The Northwest Wall and Ceiling Bureau advises against using an elastomeric coating to solve water intrusion or flashing problems.

Can you put regular paint over an elastomeric coating later?

It is possible on many products, but it is not simple. Elastomeric films are thick and flexible, and the NWCB notes they can be difficult to remove or recolor later. Any topcoat must be compatible with the elastomeric underneath, so check the manufacturer's data sheet or ask the original contractor what was used before choosing a new product.

Is elastomeric coating good for a brick house?

Usually not for a typical brick home. Brick needs to release moisture, and a low-permeability elastomeric can trap it, which can lead to blistering or damage in freezing weather. Breathable masonry paint, mineral paint or limewash are more common choices for residential brick. Elastomerics fit better on concrete block, tilt-up and some stucco walls with fine cracking.

How thick is elastomeric coating compared with paint?

Elastomeric coating is applied at a much heavier film build than standard exterior paint, which is how it bridges hairline cracks and stretches as the wall moves. The exact thickness and spread rate are set by the product's data sheet. Applying it too thin removes the benefit, so a proposal should state the product and the planned coverage.

Does elastomeric coating need a primer?

Many systems call for a masonry primer or conditioner, especially on new, chalky or patched surfaces, while some products can be applied directly on sound masonry. The manufacturer's data sheet decides. New stucco also needs to lose some of its alkalinity first, and the NWCB notes that typically takes a week to 10 days.

Sources

Keep reading